USSRPhoto.com

Soviet Photo Archive / 1926 No. 3

Tips and Recipes

Editorial board · how-to · original pages 88–89

For the summer season

Summer is coming, and with it hot weather, when amateurs and excursionists are especially busy with photography. In the heat, above all in the south, development is greatly hindered by the high temperature of the solutions, which cannot always be cooled artificially. One should therefore choose developer formulas that work without giving veil and without warping or wrinkling the gelatin layer when warm. Some recipes:

A — Amidol developer
Water1000 cc
Amidol5 g
Crystalline sodium sulfite60 g
Sulfo-ammonium salt250 g
Potassium bromide3 g
B — Metol-hydroquinone developer
Water1000 cc
Metol1.5 g
Hydroquinone1.5 g
Crystalline sodium sulfite400 g
Crystalline soda27 g
Potassium bromide2.5 g
C — Pyrogallol developer
Water1000 cc
Pyrogallol10 g
Crystalline sodium sulfite50 g
Crystalline soda135 g
Potassium-bromide solution (1:10)30 cc

As a fixer in hot weather, an acid hardening fixer can be recommended: I. Water 1000 cc, hyposulfite 250 g. II. Water 1000 cc, crystalline sodium sulfite 200 g, glacial acetic acid 150 g, ordinary alum 200 g. To prepare it, mix 20 parts of solution I with 2 parts of solution II.

Alum-hardening of negatives

In summer, when the developer is warm, one often sees the gelatin layer sliding off the glass: starting from the edges it blisters, warps and tends to come away entirely. One can still, by careful rocking of the tray, finish developing and fixing, but at the washing in running water the beginner is at a loss — could one set the negative straight to dry it would be saved, but it must first be washed, and the risk of the layer sliding grows so great that a way out must be found; sometimes, not noticing the layer starting to lift, one finds after washing a bare glass in the bath and the emulsion floating in the tank as an unsalvageable lump. So in hot weather it is always advised, after fixing and a careful half-minute rinse, to harden the negative by soaking it a while in an alum solution: 500 cc water + 50 g potassium alum, or 500 cc water + 25 g chrome alum. Chrome alum is better — it hardens more effectively. As for time, “over-holding” is harmless; usually 10–12–15 minutes suffice. My test: after a few minutes I run the pad of my index finger over the layer (under water); a squeaking sound marks the end of the process — quite safe if the finger is wet, and you soon learn to judge the degree of hardening by the sound. After hardening, washing is safe. Hardening can be combined with development and with fixing.

Simple recipe for matolein

French turpentine 100 cc, gum-dammar 5 g.

Toning baths for colouring prints on bromide-silver paper

I. Sepia tone. A: Water 1000 cc, potassium bromide 10 g, red prussiate of potash 10 g. B: Water 1000 cc, sodium sulfide 5 g. The print stays in solution A until fully bleached; after a 10-minute wash in running water it goes into solution B, where it at once takes the colour; then it is finally washed.

II. Red tones. Sepia-toned prints, after careful washing, are immersed in: Water 1000 cc, ammonium thiocyanate 25 g, tartaric acid 5 g, table salt 5 g — to which, not less than 12 hours before use, 50 cc of gold-chloride solution (1:100) is added.

III. Green tones. Prepare four solutions: A — Water 100 cc, uranium nitrate 10 g; B — Water 100 cc, ferric-ammonium citrate 10 g; C — Water 100 cc, red prussiate of potash 10 g; D — Water 100 cc, strong nitric acid 7 cc. For every 30 cc of water take 12 drops A, 12 drops B, 24 drops C, 24 drops D. After toning, the prints are washed. A more intense green can be had thus: prepare solution E — Water 100 cc, glacial acetic acid 10 cc; for the tone take B 15 cc, C 15 cc, E 150 cc; tone the print in it, rinse, and put it in solution F — Water 100 cc, chromic acid 10 cc; rinse again and put in solution G — Water 100 cc, ordinary alum 5 g; then finally wash and dry.