USSRPhoto.com

Soviet Photo Archive / 1926 No. 9

The Making of Diapositives

P. Radetsky · how-to · original pages 250–253

In winter, in the long dark evenings, the photo-amateur can occupy himself with processing the material shot during the summer period — making from the negatives prints on bromosilver paper, occupying himself with enlargement, or with the making of diapositives.

Since in our conditions diapositives are so far the most widespread and generally accessible way of illustrating various kinds of lectures and readings, the making of properly selected collections of diapositives should present an undoubted interest both for separate persons and for photo-circles conducting cultural-educational work. By the word diapositive is understood a positive photographic image on some transparent support (on glass, celluloid film, or transparent paper).

For making diapositives can serve negatives directly shot from nature, or specially made for this purpose from photographs or drawings. In No. 2 of Sovetskoe Foto we gave a description of a simple photographic installation for reproducing negatives from drawings, pictures or small objects. Now we shall dwell on the very way of making diapositives from the negatives obtained in one way or another.

Generally speaking, diapositives can be made in two ways: either by the so-called contact method — that is, direct copying from the negative in a frame — or with the help of a camera, giving the possibility of getting them in enlarged or reduced form compared with the negative. Besides, by the kind of plates used specially for diapositives, one should distinguish the preparation of diapositives printing with a visible image and with developing. In view of the undoubted advantages, in the sense of making diapositives, of the so-called chloro-bromosilver diapositive plates, which print with developing, we shall in this article analyze only the methods of work with these plates by the contact method of printing.

Thanks to the relatively insignificant sensitivity of these plates* compared with ordinary bromosilver plates, the work of making diapositives can be conducted in a dark laboratory lit with yellow light. In order that on the diapositive, in printing, black halos should not result at the edges, one should first glue the negative at the edges with black paper, or insert between it and the diapositive plate a mask of corresponding dimensions. Then the plate is placed layer to layer together with the negative into a copying frame, and one must watch that the plate be properly placed in the case where the negative is of larger dimensions. Behind the plate is placed a sheet of black or red paper, after which the frame is carefully closed with the cover and springs.

Printing is done under electric lighting. For this one can use a special copying apparatus, but it is much simpler, and perhaps even better, to use a sixteen-candle lamp, lit at a known distance (from 1 to 1.5 metres) from the frame, placed so that the light falls on it quite directly. The time of lighting depends, on the one hand, on the sensitivity of the diapositive plates, and on the other, on the density of the negative, the distance of the frame from the lamp, and especially on the composition of the developer. Depending on these conditions, it is measured from several seconds to 1–2 minutes.

The developing of diapositives

The developing of diapositive plates is conducted in the same way as the developing of ordinary plates, with the difference that by the developing of diapositives we can attain their various shades — from black to red-brown. As a general rule, one can indicate that with a short exposure and a fast-acting developer black shades are obtained, while with a more prolonged exposure, in connection with slowed developing, warm, brownish tones result. To get these shades, then, we should choose a diluted developer with a small content of alkali and with the addition of a sufficient quantity of potassium bromide.

It is not easy, properly speaking, to indicate the recipe of a universal developer equally suitable for plates of various makes and firms. In this case it is best to hold to the recipes indicated for the given sort. One can, of course, use the normal developers employed for ordinary plates, correspondingly diluting them with water and adding a certain quantity of potassium bromide; but the best results are unconditionally obtained with specially prepared solutions. As tested and most suitable developers one can point to the following.

Metol-hydroquinone developer for diapositives, in one solution:

Water1,000 cu. cm
Metol2 g
Crystalline sodium sulphite62 g
Hydroquinone16 g
Crystalline soda78 g
Potassium bromide2 g
Citric acid2 g

Hydroquinone developer for warm tones (in two solutions):

A. Water1,000 cu. cm
   Hydroquinone6.5 g
   Crystalline sodium sulphite5.2 g
   Potassium bromide0.6 g
   Citric acid0.6 g
B. Water1,000 cu. cm
   Crystalline soda85 g
   Caustic soda4 g

To make the developer, mix A and B in equal volumes. For warmer shades one can take somewhat more of solution B.

Metol-hydroquinone developer for black tones (in two solutions):

A. Water1,000 cu. cm
   Metol4 g
   Crystalline sodium sulphite34 g
   Hydroquinone4 g
B. Water1,000 cu. cm
   Potassium bromide2 g
   Crystalline soda35 g

To make the developer, mix A and B in equal volumes. The temperature of the developer should be about 21°C (17°R).

Pyrogallol developer for deep brown tones:

Water1,000 cu. cm
Pyrogallol3.5 g
Crystalline sodium sulphite14–28 g
Crystalline soda14–28 g
Potassium bromide1.7 g

For brighter shades one must take a greater quantity of potassium bromide (from 3.5 to 7 g). Developing lasts from 6 to 12 minutes. The developer gives considerable scope in the sense of exposure time, but has the essential defects of being poisonous and staining the hands and clothing.

Amidol developer (after Namias):

Water1,000 cu. cm
Metol1 g
Crystalline sodium sulphite50 g
Amidol5 g
Potassium bromide2 g

The presence of metol promotes the developing action of amidol. In case of need one can increase the quantity of potassium bromide.

In general, concerning developing, it is necessary to indicate that with any developer one should develop somewhat stronger than the diapositive should be in its final form, because in fixing it is somewhat weakened. During the work the degree of developing is determined against the light before the yellow glass of the lantern, and also by the appearance of the image from the glass side, which indicates that the developing has spread into the depth of the layer.

Properly developed diapositives are rinsed and fixed, best of all in an acid fixer composed by one of the following recipes:

Water1,000 cu. cm
Hyposulphite150 g
Potassium bisulphite25 g

or:

A. Hot water700 cu. cm
   Hyposulphite400 g
B. Hot water300 cu. cm
   Crystalline sodium sulphite70 g
   Citric acid35 g

On cooling, both solutions A and B are mixed together to get the fixing bath. The fixed diapositives are washed in the usual way and dried on racks.

The toning and colouring of diapositives

If the desired shade does not result at once by developing, then diapositives can be toned and coloured by various methods. Diapositives to be toned should be especially carefully washed free of hyposulphite; if they have been previously dried, then before toning it is useful to soak them, keeping them in running water about ¼ hour. There exists a large number of virages for colouring diapositives; of their number I shall give only some, the simplest.

Uranium virages (in three solutions):

A. Water100 cu. cm
   Uranium nitrate1 g
B. Water100 cu. cm
   Red prussiate of potash1 g
C. Water100 cu. cm
   Ferric chloride1 g
   Hydrochloric acid5–10 drops

The virages are composed as follows: I. For brown tones — 10 parts A and 1 part B. II. For red-brown tones — A and B in equal parts. III. For green tones — diapositives are immersed for two minutes in virage II and, after washing, are immersed in a virage composed of 1 part C and 5 parts water. IV. For blue tones — they are obtained by the same processing as for green tones, but virage C is not diluted with water. Since uranium virages act in an intensifying way, it is best for toning to take somewhat overexposed and underdeveloped diapositives, so that the image on them is somewhat limp.

Copper virage (after Sedlaczek):

Potassium citrate (10% solution)250 cu. cm
Copper sulphate (10% solution)40 cu. cm
Ammonium alum (saturated solution)*100 cu. cm
Red prussiate of potash (10% solution)30 cu. cm
Water750 cu. cm

The virage gives shades from red to violet-brown, with the lights remaining transparent.

Iron virage (after Sedlaczek):

Iron alum (10% solution)25 cu. cm
Potassium oxalate (10% solution)60 cu. cm
Ammonium alum (saturated solution)100 cu. cm
Hydrochloric acid5 cu. cm
Red prussiate of potash (10% solution)20 cu. cm
Water1,000 cu. cm

Cold blue tones are obtained. If, instead of the hydrochloric acid and the ammonium alum, one takes 10 cu. cm of a 10% solution of tartaric (wine-stone) acid, then grayish-blue shades result. After toning, the diapositives are washed and dried.

The colouring of diapositives is done with the help of aniline dyes. One can indicate the following simple method. Preliminary bath:

Copper sulphate7.5 g
Ammonium citrate25 g
Red prussiate of potash12 g
Ammonium carbonate4 g
Waterto 2,000 cu. cm

The indicated substances are dissolved separately in a small quantity of water, filtered through cotton wool and mixed together; then so much water is added that the total quantity of solution is 2 litres. The temperature of the bath should be about 20°C. The diapositives remain in it from 5 to 10 minutes. After a 10-minute washing in running water, they are coloured in the following solutions:

For a red tone:
Water2,000 cu. cm
Safranine2 g
Glacial acetic acid10 cu. cm
For an orange tone:
Water2,000 cu. cm
Chrysoidine0.08 g
Glacial acetic acid10 cu. cm
For a violet tone:
Water2,000 cu. cm
Methyl-violet0.08 g
Glacial acetic acid10 cu. cm

After colouring for 5–10 minutes, the diapositives are washed and dried. The finished diapositives should be mounted — but of that one can talk another time.

— P. Radetsky

* Sensitivity about 3 by Scheiner (32 by Wynne or 11 by Warnerke).   Ammonium-alum solubility: 1 part to 8.5 parts of water.