51. To I. Borzov (Sukhum). A gelatin glue for pasting prints can be prepared by the following recipe:
| Gelatin | 20 g |
| Warm water | 400 cu. cm |
On the dissolution of the gelatin, add: glycerin 2 cu. cm, alcohol 50 cu. cm. The addition to the glue of a small quantity of carbolic acid promotes its preservation. The glue must be applied warm, to dry prints. Starch glue is prepared thus: starch 1 part, water 1 part. The mixture is well ground, 4 parts of water are added, and with constant stirring it is boiled; when the solution has thoroughly boiled, 1 part of alcohol and a little carbolic acid are poured in.
52. To K. Soldatov (Kazan). There are many ways of preparing matte glasses; the simplest consists in pouring over a well-cleaned glass (one can use an unneeded negative for this) with matte lacquer. This lacquer gives a fairly fine grain and dries fast. Its recipe:
| Ether | 200 cu. cm |
| Sandarac | 18 g |
| Mastic | 4 g |
| Benzene | 50–100 cu. cm |
The benzene is added after the dissolution of the previous substances, regulating its quantity according to the desired size of grain.
53. To L. Samsonov (Vitebsk). For developing plates of various sizes, where it is conducted in little trays corresponding to the format of the plates, the following quantities of developer are needed:
| Plate 9×12 cm | 40 cu. cm |
| 12×16½ | 50 cu. cm |
| 13×18 | 60 cu. cm |
| 18×24 | 90 cu. cm |
54. To B. Limnovich (Vinnitsa). For blackening metal cassettes the following composition is used: warm alcohol 16 cu. cm, nitrate of copper 50 g. The cassette, coated with this solution, is immediately heated over a spirit lamp; if the forming black deposit is insufficient, the operation can be repeated.
55. To O. Morskoy (Orel). To give greater transparency to matte glass, its matte side is wiped with settled, beaten egg-white, or with glycerin, or with vaseline.
56. To Subscriber No. 2092 (Verkhneudinsk). The composition of an iron developer is extremely simple, and its component parts can be got everywhere:
| I. Water | 1000 cu. cm |
| Neutral potassium oxalate | 300 g |
| II. Water | 300 cu. cm |
| Ferrous sulphate (purified iron vitriol) | 100 g |
| Strong sulphuric acid | 5 drops |
In the absence of sulphuric acid, it can be replaced by citric or tartaric acid in a quantity of 1 g. The solutions are kept separately, and solution II must be kept in the light, since in darkness it quickly spoils. Just before use, the solutions are mixed, pouring one part of solution II into three parts of the first (not the reverse!). For overexposures, 2 to 10 drops of a 10% solution of potassium bromide are added to the developer. For underexposures the addition of 2–6 drops of the following solution is recommended: water 200 cu. cm, hyposulphite 1 g. Instead of adding the hyposulphite solution, the underexposed plate can be treated before developing, for one minute, in the solution: water 2000 cu. cm, hyposulphite 1 g.
57. To E. N. Laskoronskaya (Leningrad). Ink spots on a print can be destroyed by wetting the print, soaked in warm water, with a 10% solution of oxalic acid in warm water, taken on a cotton tampon.
58. To A. Kruchinin (Kostroma). The light reflected from the snow, getting from below into the lens, can veil the plate. To avoid this it is useful to put a cardboard tube on the lens.
59. To N. Hoffman (Rostov). For removing lacquer from a negative, the negative is treated with alcohol. For the fast removal of lacquer the mixture is used: alcohol 1000 cu. cm, caustic potash 20 g. The layer of lacquer clouds and can be removed with a piece of cotton wool.
60. To S. Marshtein (Kherson). For destroying hyposulphite one can use the following solutions: water 1000 cu. cm, 2% solution of potassium permanganate 10 drops; or: water 1000 cu. cm, Javelle water 15 cu. cm.
61. To V. Shimansky (Sverdlovsk). Greasy spots on prints can be removed by rubbing them with a mixture of starch and benzine. So that no traces remain on the print, it is necessary to grind the mixture of starch and benzine thoroughly, until a dry, crumbling mass is obtained.