USSRPhoto.com

Soviet Photo Archive / 1927 No. 6

Photographic Talks — Talk VII: The Treatment of the Negative after Development

A. Donde · how-to · original pages 175–180

Talk Seven of A. Donde’s beginner’s course (Talks One–Six in Nos. 1–5): fixing and washing the negative, and the correction of its defects — of gradation, veil, and non-photographic faults.

Fixing the negative

After development the negative still holds, in the half-tones and especially the shadows, unchanged bromo-silver that light could still alter, and (even after washing) active developer favouring that change — so the washed negative goes into the fixer, which dissolves the bromo-silver and leaves the silver deposit (at least during the 15–20 minutes it is in the bath; a longer stay dissolves some silver and weakens the negative). The fixing substance is “hyposulphite” (sodium thiosulphate), sold as crystals and kept ground-stoppered; in industry its power to dissolve haloid salts earns it the name “antichlor.” A 25% water solution fixes, but an acid fixer is better:

SolutionConstituents
IWater 1280 cu. cm; hyposulphite 400 g
IIWater 320 cu. cm; sulphite 80 g — then add slowly, by drops, 9 cu. cm concentrated sulphuric acid

Pour solution II slowly, in a thin stream, into I — exactly so, or caustic sulphurous gas (a poison) is released. The sale “fast-fixing salt” adds about 70–80 g of ammonium chloride per litre to solution I. Rinse the plate very thoroughly first, both to spare the fixer and because developer left in the depth of the layer later gives a two-colour (dichroic) veil. The acid fixer is handier — it almost at once stops development (which works in alkali) and keeps better. The white (light-yellow) unreduced bromo-silver dissolves away and the plate clears; but do not stop there, for the first double salt formed is hard-soluble and badly washed out — only in excess hyposulphite is a soluble, easily washed salt formed, which, if left, decomposes under the air’s carbonic acid into sulphide silver and yellows the layer. So never exhaust the fixer — keep an excess of hyposulphite, and fix no more than 50 plates of 9×12 cm per litre. Wash, in a fresh bath, at least half an hour in running water, better 1–1½ hours in running or often-changed water (a galvanized or nickelled tank, water in at the top of one end and out at the bottom of the other, the outlet fitted with a siphon tube so the tank stays full if the inflow stops); then set the plates to dry on little trestles.

Fast washing and drying

Where speed is needed (travel, excursions, hot climate, correspondent work), use salts that destroy the hyposulphite and hasten drying. Wash the plate ¼ hour in water changed three times, or running, then put it in water 100 cu. cm + 1 drop of 1:50 potassium permanganate and wash until the pink liquid stops decolorizing, followed by a short wash. To dry fast, let the water drain, then bring the plate into 90° alcohol for 10 minutes (changing it twice) — it then dries quickly (the spent alcohol can be dehydrated with pieces of gelatin, which are themselves dried for reuse); alcohol-dried plates visibly intensify. Do not dry in sun or by a hot stove (the layer melts), and do not mix fast and slow drying on one negative, as differently dried parts differ in density. As to fixing in the light: a clean, unexposed, undeveloped plate brought to the light and fixed gives a clear layer; a plate put in developer and merely rinsed blackens in the light, but one thoroughly washed (and rinsed besides with 2% tartaric acid) does not — so a well-washed developed negative may be carried out to fix in the light without harm.

Defects of the negative

A correctly exposed and developed negative is “strong, brilliant”: shadows transparent but full of detail, density rising evenly to well-covered but not opaque, detailed lights. Faulty lighting or development gives defects of gradation; a coloured coating or grey-black film is veil; further faults are of photographic, and finally of non-photographic, origin.

I. Defects of gradation

Two questions arise — was the exposure, and was the development, correct? The detailing of the shadows answers the first: enough shadow detail means the exposure was sufficient; much shadow detail with small light-shadow contrast and lightly covered lights means overexposure (a “flat” negative), while glassy, detailless shadows mean underexposure. The covering of the lights answers the second: opaque, detailless lights (and a general excess density) mean over-development. Too dense negatives are cured by weakening, too thin ones to a degree by intensification.

Weakening. The common Farmer’s reducer: hyposulphite solution 1:8 — 100 cu. cm; 10% red prussiate — 5–10 cu. cm. The image-silver turns to ferricyanide silver, which dissolves in the fixer present; it acts evenly through the thickness, somewhat raising contrast and making the negative more printable; watch it, and after enough weakening wash well to stop it. Mix it just before use (the mixture is short-lived; the 25% hyposulphite and 10% prussiate keep separately). The persulfate reducer (3–5% ammonium persulfate; Andresen’s fuller recipe: 5 g persulfate in 100 cu. cm distilled water + 4 cu. cm ammonia sp. gr. 0.91 + 2 g table salt + 50 g hyposulphite) attacks the thicker silver — the lights — more, so it softens contrast; wash and dry the negative first, leave it in till the wanted degree (the process starts as the bath turns milky), then with a simple persulfate solution put it 5 minutes in fresh hyposulphite (1:6) and wash ½ hour, or into 10% sulphite or hyposulphite to stop it (with Andresen’s, only thorough washing is needed).

Intensification. The sublimate intensifier: water 100 cu. cm, sublimate (mercuric chloride) 5 g, table salt 5 g. The dried, well-washed negative bleaches white in it (the silver turning to mercuric chloride and silver subchloride; keep the solution in the dark, reusable), then is washed and blackened in ammonia (10 cu. cm sp. gr. 0.91 in 100 cu. cm water) to a deep bluish black, and washed again — the three washings (after fixing, after bleaching, after blackening) all done thoroughly. Blackening with a sulphite solution gives durable negatives (ammonia ones are less durable, though more flexible and stronger); the strongest comes from sulphide ammonium, done under draught for its smell; iron and hydroquinone developers also serve. Sublimate is an extremely strong poison — handle it with great care and never keep it unlabelled or unmarked POISON. A non-poisonous copper intensifier: distilled water 200 cu. cm, copper sulphate 5 g, potassium bromide 5 g, table salt 15 g — treat in the dark till bleached, rinse, immerse in 10% silver nitrate, wash well (if the wash after bleaching was superficial, blacken with a developer). Intensification raises contrast, acting unevenly (lights more than shadows); a flat, too-transparent negative can be a little intensified by printing it under a red film. Quite flat negatives are best intensified with the uranium intensifier: distilled water 100 cu. cm, citric acid 2.5 g, uranium nitrate 1.0 g, red prussiate 0.3 g — colouring the negative first brown, then red (it keeps well in the dark, and long washing with weak ammonia can weaken a uranium-intensified negative again).

Systematic correction. 1. Too dense (prints slowly): a) over-development at correct exposure — weaken in Farmer’s; b) over-long exposure (not reaching overexposure) — weakening fully corrects it; c) detail in both shadows and lights but too dense overall (overexposure) — Farmer’s reduces the density, contrast steady or slightly raised; d) dense opaque lights, too contrasty (underexposure, too-concentrated developer) — weaken the lights only, with ammonium persulfate. 2. Too transparent (thin, weak): a) glassy detailless shadows, lights barely covered (underexposure) — intensification can scarcely help; b) a flat monotone negative from overexposure with development stopped too early — intensification helps, especially after first weakening to clear the shadows; c) shadows well worked but both lights and shadows weakly covered (normal exposure, development stopped early) — such negatives print well on hard papers, and intensification can make them yield strong images even on soft bromide papers. Gradation can also be much changed by re-copying the negative to a diapositive and back, repeated and regulated by lighting and development.

II. Veil

Grey veil. If it covers the whole plate, even the parts masked by the cassette frame or its hooks, the cause is either bad making and packing of the plate (very rare in foreign plates) or exposure to actinic light before loading or during development; if it spares the masked parts, the cause is overexposure, a too-warm developer, or too much alkali. A grey mourning-border along the edges is mostly seen in long-lain plates or those wrapped in impure paper, and is also laid to chemical reactions in manufacture. A reducer removes general veil, though not without touching the light half-tones; and an even general veil does not necessarily harm — on a too-thin negative it does no harm, answering to an even covering. Re-copying can help here too. Coloured veil. Yellow veil comes from too long development and a developer fouled with fixer; dichroic (two-colour: brown by transmitted, greenish by reflected light) from putting into the fixer a plate not washed of active developer. Both are destroyed by thiocarbamide: water 1000 cu. cm, thiocarbamide 20 g, citric acid 10 g.

III. Defects independent of exposure and development

Insufficient washing lets the unwashed salts crystallize in time and spoil the negative past saving. Sharply bounded darker areas mean the developer was not poured over the whole plate at once. Double contours on all objects mean the camera shook (wind, a weak tripod, a shift in hand-held work); double contours on some objects mean too slow a shutter for a moving subject, or a restless model on a time exposure. An image unsharp despite sharp focusing is more likely a cassette ill-fitted to the camera, the plate not sitting where the ground glass was, than a non-achromatic lens. Darker stripes, usually from the edges, appearing after drying come from uneven drying — the faster-dried places are darker. Black circles opposite the lens are either a light spot from shooting against the sun, or, with folding cameras, the lens opened while the camera was folded and the cassette open.

IV. Defects of non-photographic origin

From the operator’s carelessness or poorly made plates: the layer slides from bad plate-making, unequal solution temperatures (warm alternating with cold), or a too-warm, too-alkaline developer; transparent little spots come from layer defects or dust on the plate before exposure (brush it with a soft clean brush when loading); black opaque spots from particles of undissolved developer; fingerprints from touching the layer with sweaty fingers; white points on the print from dust on the finished negative, and black points from dust on the negative before exposure.

— A. Donde

(Talk Eight, “The Positive Process on Papers with Development,” in the next number.)