Developing Negatives When in Doubt of the Exposure

E. Bystrov · how-to · original pages 22

E. Bystrov on the glycin developer, which — with a simple test bath and three variant developers — can save a plate whether it was under-exposed, normal or over-exposed.

The defects of a negative are corrected by development, but the usually-applied metol-hydroquinone developer gives no wide scope in exposure, and more or less incorrectly taken exposures cannot usually be fully corrected. But there are developers giving a very wide field of exposures — these are glycin and pyrogallol. Especially glycin develops over-exposures well: in it one can get decent negatives from such exposures as in metol-hydroquinone would be irretrievably lost. I shall stop on development with glycin, as the simpler and not yielding to pyrogallol.

The developer is prepared in concentrated form thus (by Hübl’s recipe). Heat in a glass vessel 50 cu. cm of distilled water to boiling and dissolve in it 50 g of crystalline sodium sulphite; on its dissolving take it from the fire and pour in 20 g of glycin, again heat to dissolving, take from the fire and pour in 100 g of dry potash, add distilled water to 150 cu. cm — and the developer is ready. There results a grey gruel, which keeps in a bottle with a ground stopper an unlimited time. In time the liquid settling from it will colour yellow, and then black, but this does not in the least change the properties of the developer, and it is equally fit for use. Before each measuring of the gruel it is necessary to shake it strongly, and not to pour off the settled liquid. Then in separate bottles are prepared 10% solutions of potassium bromide and caustic soda. Shortly before use the following test composition is prepared: water 1000 cu. cm, gruel 12 cu. cm.1 Then a 10% solution of potassium bromide is added, in the following quantities (per 1000 cu. cm of developer): at 8–12° R — ½ cu. cm; at 12–16° R — 1 cu. cm; above 16° R — 4 cu. cm.

Into the prepared developer the plate meant for development is lowered, and the time is noted. Then one watches, by examining the plate against the light of the lantern, the appearance of the first traces of the image. If the first traces appeared 5–7 minutes after immersion, then the plate is over-exposed, and is further transferred to a developer of special composition. If the traces of the image appeared within 7–15 minutes, then the exposure was taken normal — development is further conducted in a normal developer. If after 15 minutes the traces of the image did not appear, then the plate is under-exposed, and is transferred to a bath special for under-exposures.

DeveloperComposition
For normal exposuresWater 100 cu. cm; gruel 6–7 cu. cm (if the temperature is above 16° R, add 5–10 drops of 10% potassium bromide solution)
For over-exposed negativesWater 100 cu. cm; gruel 4 cu. cm; 10% potassium bromide solution 10 cu. cm (if the over-exposure is small, one may develop simply in gruel diluted 50 times). Plates developed in this bath colour yellow, and sometimes orange, which does not affect the quality of the negative
For under-exposuresWater 100 cu. cm; gruel 2 cu. cm; 10% caustic-soda solution 4 cu. cm

Development is conducted in all cases, as usual, to the needed density; then follows a small rinsing and an acid fixing bath with alum, or a separate aluming, since the gelatin layer from prolonged development strongly softens and may be accidentally spoiled. We recommend a fixing bath of the following composition (“Aerofoto”): water 500 cu. cm, hyposulphite 150 g, crystalline sulphite 10 g, acetic acid (glacial) 10 cu. cm, chromic alum 2 g. First one dissolves all the rest, and then adds the hyposulphite.

By the described method of development one can equally well develop shots with a difference in the exposures of 500 times. So, for example, Hübl made the following experiments: at one time one and the same place was shot on three plates. The first plate was exposed 1/50 second, the second 1 second, and the third 10 seconds. After the test in the test developer, it turned out that the first was an under-exposure, the second normal, and the third an over-exposure. The negatives, developed in the developers corresponding to the exposures, gave the following results: the first and second (the under-exposure and the normal) — faultless, and the third (the over-exposure) — simply good, a little more monotone, softer than the rest. We think that photo-amateurs to whom this method of development is unknown, having tried it, will remain satisfied with it. In our practice there has not yet been a case where even one negative, which in other developers would have perished irretrievably, after development with glycin did not turn out fit.

— E. Bystrov

1 For the measuring of the developer it is very convenient to acquire a little measuring-glass of 5–10 cu. cm.