P. Wiglebe on how cold hampers every stage of the work — developer and fixer that slow or stall, solutions that crystallise, daylight papers that go flat, lenses that mist over and shutters that seize up — and how to guard against it.
The cold season has a noticeable influence on the photographic processes taking place both under the open sky and in the laboratory. At a low temperature the chemical processes proceed more slowly and less intensively than at a high one; at too low a temperature the chemical reactions may even come to a complete halt.
The action of the majority of developers depends in great degree on the temperature of the solution. A cold developer, and consequently slowed development, give too harsh negatives; with a cold developer, often development does not reach the end at all and the shadows remain transparent. The colder the developer, the later the first traces of the image appear.
The majority of developers work normally at a temperature from 16° to 19° Celsius; with a lowering of the temperature the energy of the developer also falls. This weakening of the action is not the same with different developers: with quick-working developers it is less noticeable than with slow-working ones.
Most sensitive to a lowering of temperature are the hydroquinone and the glycin developers, which at 7° of warmth already have almost no action at all. Pyrocatechin with caustic soda works satisfactorily even at lower temperatures. On the metol developer the cold has less influence. On the cooling of a metol-hydroquinone developer, the hydroquinone does not act and the metol alone works, and the results of development come out other than one might expect from a metol-hydroquinone developer.
The fixing bath at low temperatures also works extremely slowly and unsatisfactorily, giving not fully fixed and therefore impermanent negatives. In the very dissolving of hyposulphite in water its temperature falls considerably, and therefore in winter, in making up the fixer, one should use somewhat warmer water than is desirable for the ready solution.
All the other photographic solutions also work badly when cold. Weakening and intensifying baths, gold and platinum baths, cease to act at a temperature below 10°C.
The washing of emulsion papers after development or toning should be begun not at once with cold water, since a sharp change of temperature may lead to the formation of blisters; the further washing, however, can be conducted with cold water.
All the foregoing says that in the cold season one should take care to maintain room temperature in the laboratory premises. If this is impossible, then one should keep the developers and other solutions in conditions of room temperature.
Let us indicate also that substances dissolved in water, at too low a temperature, crystallise out, falling to the bottom of the vessel in the form of crystals; on subsequent heating to the needed temperature they do not always dissolve again at once. If you make up a developer from separate solutions, you must not mix them before heating, since the crystals that have separated out will not get into the mixture and the whole solution will have a composition other than you need. Besides, different substances separate out from a cooled solution unequally and unevenly.
A developer heated to the required temperature cools quickly in a cold premises; to maintain it at one and the same temperature throughout the whole time of development, one can place the little bath with the developer in another, larger one, filled with heated water or sand. The temperature of the developer is in this case checked with a thermometer, since excessive overheating is also harmful.
To print on daylight papers in winter in the open air is not recommended: daylight papers (which is especially noticeable with matte albumen papers) give flat images in the cold. If one nevertheless has to print under the open sky, then one should watch the course of the printing right there, in the cold, since if the frame is carried into a warm premises, the negative sweats over, the paper too becomes damp and may stick to the negative; and in the latter case silver spots result, which may completely spoil the negative. For this same reason, in checking a print under the open sky, one should protect both the negative and the paper from warm breath. The lacquering of negatives saves them from damp, and therefore in winter, in printing in the cold, it brings benefit. Photographic papers should be kept in a cool but not cold (and not warm!) premises.
The apparatus too suffers from the action of the cold when working under the open sky. On bringing chilled objects into a warm premises, damp noticeable to the eye is deposited on them. Especially much damp is deposited on the lens, which mists over and covers with small drops of water at each bringing in from the cold street into the room. If you have come into a premises for shooting, then the misted lens cannot give a clear image and one must wait until it warms up. Besides, many glasses are hygroscopic and in the course of time, under the influence of damp, become dull and need re-grinding, which can be entrusted only to a special establishment.
Returning from the cold winter air into a warm premises, one should wipe dry the lens and all the metal parts of the camera. The lens should be wiped both in front and behind with a clean soft rag (not chamois!).
Damp is deposited not only on the outer surface of the lens, but sometimes inside it too, and also inside the shutter, whose modern precise models are very delicate. The speeds of action of shutters under the influence of cold and damp noticeably diminish; in a strong frost some focal-plane shutters cease to work altogether. Therefore, when working in a frost, it is useful to warm with the hand the parts of the shutter projecting outward (but by no means the lens!).
Cassettes with plates it is useful in winter to carry in the warm pockets of one’s clothing.
— P. Wiglebe