N. D. P. on working through the hot summer, when the temperature of the solutions decides the character of the negative. Cooling the developer with ice; a borax metol-hydroquinone developer and an acid amidol developer that resist fog and flaccidity; tanning the layer with chrome-alum against the wrinkling of the gelatin; a tanning acid fixer; and a thymol bath against the bacteria that breed in slowly-drying gelatin.
On hot summer days photographers often experience very significant difficulties in the getting of a good negative. At such a time of year only the observance of special conditions at work and general attentiveness can protect them from an excessively large quantity of rejects. All chemical processes, as is known, depend on temperature; in the laboratory practice of the photographer the temperature of the developing, fixing and other solutions has a decisive significance in the getting of this or that character of negative.
Development
Since in the summer months the temperature of the developing solutions often is higher than normal (above 18° Celsius), the process of the restoration of silver bromide in these conditions proceeds relatively faster — the developing bath works the more energetically the higher the temperature of the solution. In these cases negatives can come out not only soft but sometimes simply flaccid; besides, the higher — compared with normal — the temperature of the developing bath, the greater the danger of the formation of fog on the negative. The latter especially tells at the development on hot days of plates of the highest sensitivity.
The first measure, suggesting itself, is the cooling of the developing solution with ice: either by placing the bath with developer in ice, or by cooling it by the direct dissolving of ice in the developer. Besides this, in photographic literature there are special developer recipes adapted for work both in countries with a hot climate and in general in conditions of high temperature. The below-indicated recipe of metol-hydroquinone developer, at a bath temperature above normal (20–21° Celsius), gave us a quite clean and by character normal negative (at a normal exposure):
| Water | 1,000 cu. cm |
| Metol | 2 g |
| Anhydrous sodium sulphite | 10 g (or crystalline 20 g) |
| Hydroquinone | 5 g |
| Borax | 20 g |
Borax, solutions of which have a definitely alkaline reaction, as it were replaces here the alkali. Besides, borax acts in this recipe as a retarder of the process of developing the latent image. Since borax (boric-acid sodium Na2B4O7+10.H2O) dissolves extremely badly in cold water, it should be dissolved first separately in hot water (at the rate of 1,000 cu. cm) and, on cooling, added to the solution of the rest of the substances.
The wrinkling of the layer at the edges of the negative is an almost usual phenomenon, as a result of the increased temperature of the solutions. This unpleasantness especially makes itself known at a large content in the developer of alkali (soda or potash). Therefore at composing the developer one should avoid an excessive addition of soda or potash, somewhat sacrificing in this case the restoring capacity of the developer. With caustic alkalis one must be especially careful in these conditions. Sometimes, perhaps, it will be more advantageous to take such a developing substance as can work without the presence of alkali, always softening the negative layer. In this respect the amidol developer presents the greatest advantage. Of the number of amidol developer recipes it is better to take the “acid”:
| Stock solution | |
| Water | 1,000 cu. cm |
| Crystalline sodium sulphite | 200 g |
| Potassium metabisulphite | 25 g |
The amidol developer, as is known, does not preserve, and therefore the developing bath is prepared just before use, using for this the well-preserving stock solution:
| Water | 1,000 cu. cm |
| Stock solution | 200 cu. cm |
| Amidol | from 5 to 7 g |
The developer works very fast. As a means against fog, and also for the slowing of the development process, the addition of a 10% solution of potassium bromide is admissible: in the first case a few drops, in the second a significant quantity. In the hot time of year, when the danger of the softening of the gelatin layer of the negative is great, into the solution of amidol developer one can add chrome-alum in powder at the rate of up to 8 g per 1,000 cu. cm of bath, producing thus the tanning of the negative. The majority of developing substances (except glycin), possessing in one or another degree an affinity to oxygen, oxidise in the developing solution; at this the products of oxidation to some degree tan the gelatin layer of the negative. In this respect pyrogallol (pyrogallic acid) should be placed in first place, wherefore its application as a developer is also advantageous in the hot time of year.
Fixing
Unpleasantnesses can be also in the process of fixing the negative. Precisely in this period of its processing, even at a normal temperature of the fixing bath, in summer the wrinkling of the layer at the edges can arise. The only salvation in this case can serve the introduction into the fixer of this or that gelatin-tanning substance (chrome or ordinary alum or formalin). The following acid tanning fixer works rather long:
| Water | 1,000 cu. cm |
| Anhydrous sodium sulphite | 25 g |
| Tartaric acid | 10 g |
| On dissolving, add: Hyposulphite — 250 g | |
| Finally pour in the separately-prepared solution: Water 100 cu. cm, Chrome-alum 15 g | |
Washing and drying
If the layer of the negative was not subjected to tanning in the fixing bath, then its wrinkling can occur also in the wash-water. To avoid this, it is desirable that the temperature of the wash-waters should be identical and approach normal. If the washing is done in running water, then the speed of its movement should not be great.
The process of drying the gelatin layer in summertime is also subject to dangers. From bacteriology it is known that gelatin is an excellent medium where bacteria quickly and in significant quantity multiply. At the comparatively slow drying of the negative in premises without access of fresh air, in the layer of the negative forms a number of round points of a greyish-dark colour — a sign of the beginning of the formation of bacteria in the gelatin. To avoid this, the negative is recommended after washing to bathe 2–3 minutes in a water solution (½%) of thymol, again wash, and set for drying.
Among the laboratory failures of the summer works of the photo-amateur, much should be attributed to his not accounting for those circumstances which arise under conditions of high temperature in the hot time of year. Let the foregoing help the photo-amateur to ponder over this not-unimportant question — this will protect him from excessive rejects.
— N. D. P.