The eighth and last of the year’s “Step by Step” talks, the printing counterpart to No. 8’s negative-faults table: twenty-nine failures of the positive process — on daylight (printing-out) papers and on developing papers alike — each with its cause and, where worthwhile, its cure; prevention favoured over correction, since a bad print is better remade than mended. It closes the beginners’ series (to resume next year as a second stage) with six pieces of advice: blame your own hands first, don’t demand more than the camera can give, stick to one plate / developer / paper, don’t chase speed, and above all don’t skimp on the hyposulphite.
In our previous “Talk” we examined the defects of shooting or subsequent processing noticeable already on the negative; the defects of a print proceeding from not-fully-sound negatives we shall therefore now almost not touch. As for the defects of positives, their correction is for the most part completely inexpedient or even impossible, and it is far more expedient, having clarified the cause of a defect, to make a new print. So in the present talk we shall speak mainly not of correcting unsuccessful prints, but of preventing defects at their making. We proceed from the supposition that the negative is sharp and good.
Defects at work on papers with a visible image (“daylight”)
1. The outlines and lines are doubled. The paper or negative was shifted while the print was examined in the frame.
2. The whole print is unsharp, blurred. The negative lay in the frame wrong side — glass to the paper, emulsion outward.
3. The print is unsharp in some places. Negative and paper did not lie closely together (uneven frame or weakened lid-springs); the loosely-pressed places came out unsharp.
4. The print is “flaccid.” (a) The negative was flaccid or thin (see No. 8, “Talk Seven,” defects 5 and 7); (b) it was printed in direct sunlight. Prevention: for (a) strengthen the negative; for (b) print in weakened daylight (cover the frame with tissue, matte glass or yellow paper). Less flaccid prints come on a more contrastly-working paper.
5. The print is too hard. The negative was hard (see “Defects of the negative” 3). Prevention: (a) weaken the negative; (b) print in strong direct sunlight.
6. The lights (white places) are foggy, dull, unclean over the whole print. The paper was prematurely acted on by light — “fogged.”
7. The lights are dull only on one half. During printing the frame opened too often, too long, or in too strong light (the opened half was fogged). Prevention: control the image as quickly as possible and in weak light (in the depth of the room, not in the sun).
8. The tone (colour) is uneven. (a) Too little toning-fixer in the cuvette, covering the print unevenly; (b) the cuvette was little rocked.
9. The print tones too slowly in the toning-fixer. (a) The solution is too cold, or old and exhausted; (b) the paper is old. Correction: warm the solution; add fresh toning-fixer.
10. The print has ugly greyish-green tones. (a) The toning-fixer is too old or exhausted; (b) the toning went on too long and went too far.
11. Reddish-brown spots (finger-marks). The print was taken before processing with dirty greasy fingers — especially noticeable on matte papers.
12. Yellow spots. Before toning the print was taken with fingers dirtied with fixer.
13. Cracks on the sensitive side. (a) The top of the paper was bent too strongly during control — do it carefully; (b) the paper is old and its layer hardened.
14. A finished print, with time, fades or grows pale, wholly or in places. (a) Insufficiently fixed or insufficiently washed from fixer; (b) the toning-fixer was exhausted by long use; (c) if pasted on a mount, it may discolour from acids in the glue or card; (d) it was kept in an unfavourable place (e.g. a damp wall).
Defects at work on papers with development
15. The print is too pale, weak. (a) Printed too little (insufficient exposure); (b) development stopped too early (under-developed); (c) the developer was too cold or exhausted.
16. The print is too dark. (a) Printed too long (over-printed); (b) too-warm developer; (c) over-developed.
17. The print is flaccid. (a) Over-printed; (b) the negative is flaccid (see “Defects of the negative” 5). Prevention: for (b) print on contrastly-working paper (see Photo 1).
18. The print is too rich in contrasts. (a) Under-exposed, then developed longer than needed; (b) the paper is too contrasty for the negative; (c) the negative is too contrasty (see defect 3).
19. The print has a violet-grey colouring in places. Uneven fixing: not the whole print was immersed in the fixer.
20. The print has a yellowish colouring. (a) Developed in an exhausted developer, coloured by oxidation products; (b) the fixer was polluted with developer brought on insufficiently rinsed prints. Correction: fix again in fresh acid fixer for 15 minutes, then wash thoroughly.
21. The print has a greenish shade. (a) Over-printed; (b) too much potassium bromide in the developer.
22. Thin lines like pencil strokes (mainly on glossy papers). The paper rubbed against the packing at extraction from the packet. Correction: wipe the dry print with cotton moistened in spirit.
23. Small black specks. The developer contained undissolved particles which settled on the print. Prevention: dissolve substances thoroughly; if particles remain, filter the solution (Fig. 2).
24. Round, white, sharply-bounded points and spots. Air bubbles formed at the careless lowering of the print, barring the developer. Prevention: put the print in an empty cuvette and douse it with developer at once; dip it layer-down, move it back and forth two or three times, then turn it layer-up; remove any remaining bubbles at once with cotton.
25. The sensitive layer comes away from the base in bubbles (most often in the wash-water after fixing). (a) The paper is inclined to form bubbles (especially handicraft papers made in warm season without cooling devices); (b) the paper was crumpled or cracked during washing. Correction: small bubbles dry up by themselves; large ones, after washing, are pricked from the paper side with a fine needle and pressed out.
26. The finished print fades after some time. (a) Insufficiently fixed; (b) the fixer was old and exhausted; (c) insufficiently washed after fixing; (d) if pasted on a mount, acid in the glue or card.
27. The print has a grey veil over its whole area. (a) The paper is old or kept damp; (b) the red laboratory lighting is faulty and acts on the paper during development; (c) the print was subjected too long, or at too close a distance, to the red light.
28. Dark spots on the print. (a) Insufficient rinsing after development before fixing; (b) in the fixer the prints stuck together, and the developer particles remaining in their emulsion continued to act.
29. Dark and light places of irregular form. The developer, at the lowering of the print, covered it insufficiently quickly or unevenly, and acted on different places a different time (often when there is little developer in the cuvette).
Several pieces of advice
The series of very popular talks for beginners is finished. Let us hope that comrades not yet acquainted with photography managed to assimilate from them some practical skills, and — with attentive attitude to what is written and the fulfilment of all the indications — could more or less satisfactorily carry out the basic processes: shooting, development, printing. The responses the talks called forth, especially among comrades in the remote corners of the Union where no instructor can be found, and the reviews of a number of public organisations, prompt us to continue and develop the section further. The future “Talks with Beginners” (which the journal will continue next year) will be a second stage for those acquainted with photographic methods through the eight talks of this year, developing and explaining separate questions of the themes already touched; we turn to comrades who passed the first stage with the request to report what was insufficiently clear, what they did not find and would like to see. For now, several pieces of advice useful for every beginner:
- If you do not at once get satisfactory results, do not blame the apparatus or materials, but try to find the cause of the failures in your own actions.
- One cannot demand of the apparatus more than its construction and price allow. If the shutter’s maximum speed is 1/100 second, you cannot get good shots of fast movement (sport) up close; with a lens of F/11 you cannot make momentary shots in overcast weather; with F/8 you should not try momentary shots in a room.
- Do not keep rushing from one material to another. Get used to one sort of plate, one developer, one paper — having worked with them and studied them, you will more easily attain satisfactory results.
- Do not chase highly-sensitive material: the more sensitive the plates, the harder to process; likewise, a beginner gets better prints not on highly-sensitive bromo-silver paper but on gaslight paper — one has to wonder our amateurs have not yet grasped this.
- Do not economise too much on chemicals, nor use them to full exhaustion; they are not so dear that such false economy is worth spoiling correctly-shot plates (exhausted developer) and good negatives and prints (exhausted fixer). Most of all, fear economy on hyposulphite!
- Carry out all photographic processes consciously; it is useful to read books on photography.
[Figures: Photo 1 — one must be able to choose the paper to suit the negative; even a seemingly spoiled (over-exposed and fogged) negative can give a good print on a well-chosen paper — left, on ordinary normal-working bromo-silver paper; right, on hard-working gaslight paper. Fig. 2 — impure solutions, with small particles floating in them, should be filtered.]